Selective laser melting (SLM), an additive manufacturing process mostly applied in the metal material field, can fabrica......
Effect of the withdrawal rate on the microstructure and thermal durability of a third-generation sin
Single crystal Ni-based superalloys are the typical structural materials for high-pressure turbine blades, and their mic......
通过750℃低周疲劳试验,研究55Ni?23Cr?13Co基高温合金在应变幅度为0.35%~0.6%下的循环变形行为及显微组织演变.Coffin?Manson?Basqui......
The effects of substituting Co for Fe on the microstructure and stress rupture properties of K4750 alloy were studied.Th......
Rapid oxidation takes place both in the laboratory and in industrial conditions when alloy 925 is contaminated by oxide ......